Bonding PC membranes to glass
2002-04-12
Troy Plattner
Bonding PC membranes to glass
Troy Plattner
2002-04-12
We are currently trying to form a high-yield process
for bonding polycarbonate membranes to glass samples.
Our current method consists of mounting them onto PDMS
with alcohol, etching the surface with oxygen plasma
and then attempting to transfer them onto the glass
slides (which are prepared with adhesion promoter) at
a high temperature.

The main problem is getting the membrane to transfer
completely, as the PDMS still pulls on the membrane
when we try to dismount it from the glass.  Does
anyone have any related experience/suggestions?

Thanks,

Troy Plattner
Yahoo! Tax Center - online filing with TurboTax
http://taxes.yahoo.com/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.