MEMSnet Home: MEMS-Talk: re:Cracks of SU-8 mold
re:Cracks of SU-8 mold
2002-04-16
[email protected]
anti-protein coating for PDMS
2002-04-16
[email protected]
re:Cracks of SU-8 mold
[email protected]
2002-04-16
Hi Xinyu Li,

Yes! Su8 is a good for molding but just for a limited amount of time. You can
use hydrophobic coatings on the su8 before and everytime you put the PDMS. Also
you can improve the adhesion of your SU8 structures to the substrate where the
su8 was spun by using the SU8 realese layer from Microchem Corp. in Newton, MA,
USA.

good luck!
Gabriela

Gabriela Juarez-Martinez
Dept. Electronics
Rankine building
University of Glasgow
Glasgow G12 8LT. UK

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group
Harrick Plasma, Inc.