MEMSnet Home: MEMS-Talk: photoimageable insulator
photoimageable insulator
2002-05-03
Martin O. Patton
2002-05-07
shay kaplan
2002-05-07
___
2002-05-08
carlton watson
2002-05-06
Bill Moffat
2002-05-08
Greg Miller
2002-05-09
carlton watson
photoimageable insulator
carlton watson
2002-05-09
Hope you read my earlier posting. I just want to
clarify that PI2771 is a negative tone polyimide.
There is a positive series called HD-8000. You can
find an article at:
http://www.dupont.com/corp/news/product/2001/pn07_16_01a.html




--- Greg Miller  wrote:
> Are their any positive resist out there similar to
> BCB & PI that are
> positive - because currently I use BCB & PI - but I
> finding limitation
> that a positive resist would solve -
> Thanks,
>
> Greg Miller
> KVH Industries
> Email: [email protected]
>
>


=====
Carlton C. Watson, Ph.D.
Microfabrication Manager,
TLC Precision Wafer Technology
1411 West River Road N.
Minneapolis, MN 55411
Ph:  (612) 341-2795
Email: [email protected]
Yahoo! Shopping - Mother's Day is May 12th!
http://shopping.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group