MEMSnet Home: MEMS-Talk: The Temperature of DRIE
The Temperature of DRIE
2002-05-15
Jia Zhou
2002-05-15
tangyz
2002-05-15
Rick Williston
2002-05-15
___
2002-05-15
Jeff Zahn
2002-05-15
___
MEMS Rotary motors
2002-05-16
Robert Dean
2002-05-15
[email protected]
2002-05-15
[email protected]
The Temperature of DRIE
Jeff Zahn
2002-05-15
The DRIE temperature was measured at Carnegie Mellon
university MEMS lab (www.ece.cmu.edu/~mems) by xhu zhu
using a heat sensitive color change tape which
indicates the warmest temperature.

I do not know the exact protocol used but I was told
that the wafer stayed below 60 degrees. I do not think
this data was ever published.

Jeff

--- Rick Williston 
wrote:
> I find this hard to believe, how did they measure
> it?  Do you know or is
> there someone I can contact?
>
> Rick
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On
> Behalf Of tangyz
> Sent: Wednesday, May 15, 2002 7:47 AM
> To: [email protected]
> Subject: Re: [mems-talk] The Temperature of DRIE
>
>
> Hi,
>      STS confirms the temperature on the top of the
> wafer is below 60
> degree.
> good luck
>
> ----- Original Message -----
> From: "Jia Zhou" 
> To: 
> Sent: Wednesday, May 15, 2002 8:20 PM
> Subject: [mems-talk] The Temperature of DRIE
>
>
> > Who knows the temperature in DRIE when silicon is
> deep-etched, say
> 500microns?
> >
> > Thanks.
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe
> or change your list
> > options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> > Visit us at http://www.mems-exchange.org/
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.mems-exchange.org/
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.mems-exchange.org/
LAUNCH - Your Yahoo! Music Experience
http://launch.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.