        hello everyone:

I am working on a surface micromachined device with an exposed Au layer.
I was wondering if anyone knows of a low stress adhesion layer that
can withstand a long (3 hours+) HF release process.  Any papers and any
pointers are truly welcome,
Thanks,

                                                        -Mehmet
ps: MUMPS handbook uses Cr/Au however their soak times are much shorter.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.
Process Variations in Microsystems Manufacturing