metal with HF?
Michael Pedersen
2002-05-22
We have tried Cu and it does not seem to be affected by HF. Ti dissolves
in HF...
Michael Pedersen
The MEMS Exchange

Jing Liu wrote:
> To who may concern,
>
> Does anyone know whether thin coated film of Cu could resist concentrated HF
> etching? How about other metal like Ni and Ti? Are there any reference I could
> find?
>
> Jing
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/


--
MEMS-Exchange
Corporation for National Research Initiatives
1895 Preston White Drive, Ste. 100
Reston, VA 20191-5434

Phone:  703-262-5342
Fax:    703-262-5367
e-mail:
[email protected]
Please visit us @: www.mems-exchange.org

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing