lift off problem
2002-09-03
Sungjun Lee
2002-09-04
W.H. Teh
lift off problem
W.H. Teh
2002-09-04
I do it in acetone at room temperature and no problem. Make sure the
thickness of your metal is about 1/3 (better still less) than the thickness
of the PMMA resist.

WH

On Sep 4 2002, Sungjun Lee wrote:

> Does anyone who knows about the lift-off of PMMA? I have usually done it
> under boiling Acetone. Is there any difference of behavior under between
> pure Acetone and boiling? By the way, I welcom to receive any comment
> about the lift off method. Thanks in advance.
>
> S. Lee / Graduate Student
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation
University Wafer