MEMSnet Home: MEMS-Talk: How to make PDMS more hydrophobic?
How to make PDMS more hydrophobic?
2002-12-09
Xinyu Li
2002-12-10
Bill Moffat
How to make PDMS more hydrophobic?
Xinyu Li
2002-12-09
Dear colleagues,

Do you know how to make PDMS more hydrophobic?

Thanks.

Xinyu Li


reply