MEMSnet Home: MEMS-Talk: Copper film etching solution
Copper film etching solution
2003-01-10
[email protected]
2003-01-13
[email protected]
N or P type SOI choice !?
2003-01-14
sou zou
Copper film etching solution
[email protected]
2003-01-10
Hi there
I want to use FeCl3 solution to etch copper film with thickness 200nm. Does
sombody know what is the concentration of FeCl3, or any other good etching
solution for copper film. Thank you.