MEMSnet Home: MEMS-Talk: Photoresist 1818!
Photoresist 1818!
2003-01-13
Tieying Jiang
2003-01-14
Oray Orkun Cellek
2003-01-28
张振峰
2003-01-28
Mahesh Pitchumani
Photoresist 1818!
Oray Orkun Cellek
2003-01-14
Dear Jiang,

If you are in Europe you may try www.microresist.de for Shipley S1818 with
the suggested metal ion free developer of Shipley MF319.  Promoter
suggestion depends on the underlying substrate I guess.

Best regards,

Oray Orkun Cellek
[email protected]
Research Assistant, Ph. D. Student
Electrical & Electronics Engineering Department
Middle East Technical University
06531 Ankara
Turkey
Tel : +90 312 210 4579
Fax : +90 312 210 1261

----- Original Message -----
From: "Tieying Jiang" 
To: 
Sent: Monday, January 13, 2003 4:37 PM
Subject: [mems-talk] Photoresist 1818!


> Dear ALL,
>
> I am looking for photoresist 1818 (Shipley) urgently. Could anyone kindly
> give me some quick info about how to purchase it and the promoter and
> developer? Thank you very much.
>
>
>
>
>
>
>
> _________________________________________________________________
> Protect your PC - get McAfee.com VirusScan Online
> http://clinic.mcafee.com/clinic/ibuy/campaign.asp?cid=3963
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Harrick Plasma, Inc.