MEMSnet Home: MEMS-Talk: Electroless Cu-plating on SiO2 powder
Electroless Cu-plating on SiO2 powder
2003-12-05
vidya_iitk
2003-12-05
Amrit Panda
2003-12-08
Zhimin J Yao
Electroless Cu-plating on SiO2 powder
vidya_iitk
2003-12-05
Dear Sirs,


I am doing experiment to study the behaviour of electroless Cu plated sintered
Sic and SiO2 powders. I am able to do electroless plating of Cu on SiC but
finding difficulty to electroless plating on SiO2 powder. Could you please help
me in this regard.


Thanking You.


Galphade V.S.


Lecturer in Metallurgy


Govt. College of Engg. Pune, INDIA 411005

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing