MEMSnet Home: MEMS-Talk: Electroless Cu-plating on SiO2 powder
Electroless Cu-plating on SiO2 powder
2003-12-05
vidya_iitk
2003-12-05
Amrit Panda
2003-12-08
Zhimin J Yao
Electroless Cu-plating on SiO2 powder
Zhimin J Yao
2003-12-08
Galphade,

Electroless plating is an electro-chemical reaction that only happen on a
conductive surface.  There are ways to deposit a thin layer of metal film
on non-conductive surfaces buy immersing parts into solutions.  You can
find a lot information in some old books on plating.

Good luck

Z. Yao



                      "vidya_iitk" 
                      Sent by:                                          To:
                      mems-talk-bounces+zjyao=rsc.rockwell.com@         cc:
                      memsnet.org                                       Subject:
[mems-talk] Electroless Cu-plating on SiO2 powder


                      12/05/2003 03:08 AM
                      Please respond to vidya_iitk; Please
                      respond to General MEMS discussion





Dear Sirs,


I am doing experiment to study the behaviour of electroless Cu plated
sintered Sic and SiO2 powders. I am able to do electroless plating of Cu on
SiC but finding difficulty to electroless plating on SiO2 powder. Could you
please help me in this regard.


Thanking You.


Galphade V.S.


Lecturer in Metallurgy


Govt. College of Engg. Pune, INDIA 411005
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/








reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation