MEMSnet Home: MEMS-Talk: teflon glue...
Photoresist for Patterning Aluminum
2004-10-05
Vivek Mukhatyar
2004-10-05
Shay Kaplan
teflon glue...
2004-10-05
Venkatachalam Chokkalingam
2004-10-05
William Lanford-Crick
2004-10-05
aasutosh dave
2004-10-05
rakesh babu
photopatternable silicone biocompatibility
2004-10-06
[email protected]
2004-10-05
Bill Moffat
teflon glue...
Venkatachalam Chokkalingam
2004-10-05

hai,

do someone know how to paste 2 pieces of teflon? is there any specific glue for
teflon?? even if u have some other ideas, please share it..

Venkat.


Shay Kaplan  wrote:
maybe you should try phosphoric acid instead?
shay

Vivek Mukhatyar wrote:

>I was trying to spin coat aluminium with shipley 1818 negative resist.
> But when I used a wet etching solution the resist wasn't able to
>withstand the etchant. My patterns are on the scale of microns and
>the best way to etch is through wet etching because i need to remove
>alomost 300 micron thick aluminum. Does anyone know the steps to spin
>a thick layer of resist that will withstand the etchant that is made
>up of Hcl and CuCl2. I have SU-8 and 1818 to my disposal. I also
>need to remove the resist after the etching process.
>
>Thank you,
>
>Vivek Mukhatyar
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
>

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


---------------------------------
Do you Yahoo!?
Take Yahoo! Mail with you! Get it on your mobile phone.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review