Photoresist pattern on PDMS
Z.,W.Y.(Lydia)
2005-01-05

Hi, Zeng,

I had the same problem (cracks on PR) before. Even though I do not why you
need deposit PR on PDMS (I used Sylgard 184, Dow Corning), I would like to
suggest the following solutions for you consideration.

(1) You can deposit a thin Al (~800A or less) on top of PDMS, and use Al as a
masking layer.

(2) For my own experience, you might want to try the photopatternable-silicone
(Wl-5000, Dow Corning). There are much easier to process. I had a paper for u
reference.
http://www.lehigh.edu/~wez6/LEHIGH_EUROSENSORS_ESCW.pdf

Anyway, 3-5 um is very challenged for either solution.

Good luck!

Lydia











Quoting Hongjun-ECE :

> I'm trying to pattern photoresist on the PDMS but got the following
> problems. Can you guys kindly help me fix them?
>
> 1. I spined PR1818 on the PDMS but found there are a lot of thin cracks in
> the photoresist after the softbake. I guess it is caused by the difference
> of thermal coefficients between the photoresist and the PDMS. Did you guys
> have this problem and how did you resolve it?
>
> 2. I want to pattern photoresist on PDMS with a feature size of 3-5um, do
> you think it is possible? I plasma-treated the PDMS before coating
> photoresist and it seems the adhesion of the resist on the PDMS is very
> good, but when the exposed wafers are developed, all the lines with width
> less than 10um flaked off the PDMS substrate.
>
> Thanks you very much for you help,
>
> Hongjun Zeng, PhD
>
> Microfabrication Application Laboratory (MAL)
> University of Illinois at Chicago
> 3014 ERF Building, 842 W. Taylor Street
> Chicago, IL 60607
> Tel. 312-413-5889, Fax: 312-996-6465
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>




-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics