MEMSnet Home: MEMS-Talk: Photoresist pattern on PDMS
Photoresist pattern on PDMS
2005-01-04
Hongjun-ECE
2005-01-05
Z.,W.Y.(Lydia)
2005-01-19
Miao LIU
2005-01-20
Hongjun-ECE
wafer bonding
2005-01-20
li cai
2005-01-21
Hongjun-ECE
2005-02-03
Miao LIU
Photoresist pattern on PDMS
Hongjun-ECE
2005-01-20
I found if you just leave the resist-coated wafer dry in room temperature in
stead of prebake, the crack would be less or even disappear. The room dry
photoresist is still OK for the following litho process.

Just curious, how much is the smallest size do you want to pattern the
resist on the PDMS? And how is it working?

Good luck,

Hongjun Zeng, Ph.D
Microfabrication Application Laboratory (MAL)
University of Illinois at Chicago

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review