MEMSnet Home: MEMS-Talk: vendor for KOH bath
vendor for KOH bath
2005-03-15
Danielq k
cryocoil
2005-03-15
Andrew Xiang
2005-03-16
Brent Garber
2005-03-16
Andrew Xiang
vendor for KOH bath
Danielq k
2005-03-15
Hi all
 I am in the market looking for this.  Anyone know good vendor of KOH
bath. My requirements are reflux condensor cap, auto injection of IPA
and water, agitation, thermal stability.
Thanks
Daniel

reply