MEMSnet Home: MEMS-Talk: cryocoil
vendor for KOH bath
2005-03-15
Danielq k
cryocoil
2005-03-15
Andrew Xiang
2005-03-16
Brent Garber
2005-03-16
Andrew Xiang
cryocoil
Brent Garber
2005-03-16
Andrew,

I think you may be speaking of a miesner trap.  You only put LN2 in it
after you are under high vacuum to gather water out of your system.  It
does not provide pumping, but will lower you pressure a bit.  It must be
completely warmed up before venting you system.

I hope you are not talking about a cold trap needed on a system with a
diffusion pump.  That needs to be filled before opening you high vac valve
to prevent oil vapor from getting into your chamber.

Brent

Andrew Xiang wrote:
> Anyone used cryocoil to speed up the vacuum pump down?
> Do I just fill it up with LN2? Never used it and don't have experience.
> I guess it will consume a lot of LN2.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering