Question for Copper Etching
2006-06-08
Yi Yao
wafer heaters
2006-06-12
biplab roy
wafer heaters
biplab roy
2006-06-12
Dear All,
  I need to build a wafer heating system upto 200C. For that I need  flexible
thin heaters  (one I have seen, coils embedded in  polymeric substrate). I don't
know the name of that kind. Could anyone  please help me with the name of
heaters of that kind and if possible  with the availabilty.
  Thanks,
  Biplab

Yi Yao  wrote:  Hi All,

I'm planning to do copper etching on micro features (the copper will be
approximately 2um in thickness, 20um in width and 200um in length).
For some reason, I must use sulfuric-peroxide etchant. Can anyone recommend
me some commercialized etchant (sulfuric-peroxide)
for micro copper etching? I tried Fisher and Transene, but didn't find any.
BTW, generally, it is a mixture of 96% sulfuric and 30% hydrogen peroxide
with some stablizers. It will also be very helpful if someone
can give me a clue on what kind of stablizers I should use, so that I can
make the etchant myself.

Thanks a lot and your help will be highly appreciated.

Best Regards,
Yi
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk


 __________________________________________________
Do You Yahoo!?
Tired of spam?  Yahoo! Mail has the best spam protection around
http://mail.yahoo.com
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group