MEMSnet Home: MEMS-Talk: wet etch recipe for Iridium (Ir)
wet etch recipe for Iridium (Ir)
2007-01-28
Mantavya <Manu> Sinha
2007-01-29
David Nemeth
2007-02-11
Mantavya Sinha
2007-02-21
Mantavya Sinha
2007-02-22
David Nemeth
2007-01-29
Mantavya Sinha
wet etch recipe for Iridium (Ir)
Mantavya Sinha
2007-01-29
hi guyz,
can anyone tell me the wet etch recipe for Iridium (Ir). It seems to be
quite resistive to hot(85'C) dilute(1:1) aqua regia. Also the etchant
should have high selectivity over IrSi.
Looking forward to hearing from you people.

Warm Regards,
Mantavya
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMS Technology Review