A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS Sealing over Au?!
PDMS Sealing over Au?!
2007-06-21
N H
2007-06-22
shay kaplan
2007-06-22
N H
2007-06-22
Joseph Grogan
2007-06-25
N H
PDMS Sealing over Au?!
Joseph Grogan
2007-06-22
Someone can correct me if I'm mistaken, but I don't think you'll ever
get PDMS to bond to Au in the same way it bonds to glass, ti or cr. When
you plasma activate PDMS it will bond to oxides, and since Au doesn't
oxidize significantly, you probably won't be able to bond to it. I
haven't tried it myself, but I imagine ITO (indium tin oxide) would be a
good material to use as an electrode for PDMS to bond to.
-Joe Grogan

N H wrote:
> At first: Thank you very much for your kind mail Mr. Kaplan.
>
>    As the matter of fact, I had done like your suggestion before
> sending my former message, and the sealing was very good, but the
> electrode was not active anymore. I tried to etch the Ti layer on
> active Au area, but PDMS did not work very well as "mask" and I had
> lost the control  over electro's active area again, by under-etching.
> By its turn, any solution involving alignment is forbidden, since in
> my process I have no chance to settle PDMS channels over the glass
> plate with that great precision.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Nano-Master, Inc.