MEMSnet Home: MEMS-Talk: Problem with DC Sputter
Problem with DC Sputter
2007-08-02
saravan kallempudi
2007-08-02
Brent Garber
2007-08-02
Jim
2007-08-02
Birol Kuyel
Problem with DC Sputter
Birol Kuyel
2007-08-02
May have overheated the magnetron and loose the magnetic field strength of
of your permenant magnets

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of saravan kallempudi
Sent: Thursday, August 02, 2007 6:55 AM
To: [email protected]
Subject: [mems-talk] Problem with DC Sputter


Dear Members,

I have a problem with my DC sputter. We used to sputter Nickel but we have
strange problem now having plasma inside chamber but unable to sputter
nickel. I thought of target poisoning and I cleaned the target with
Nitricacid and then also I was not able to move forward. Can anyone suggest
me in this!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing