Gold Etchant with selectivity over Mo
Moshe
2008-07-23
I know that Aqua Regia may etch gold but I don't know what it influence on the
Mo.
Aqua regia composition : 25% concentration  HNO3 + 75% concentration    HCl
It is very corrosive solution, please be careful!
reply