MEMSnet Home: MEMS-Talk: Gold Etchant with selectivity over Mo
Gold Etchant with selectivity over Mo
2008-07-21
Chong Xie
2008-07-23
Moshe
2008-07-23
Kevin Paul Nichols
Gold Etchant with selectivity over Mo
Kevin Paul Nichols
2008-07-23
Aqua Regia will also etch Mo. You'll be left with a thin film of transparent
MoO3.

- Kevin

Kevin Paul Nichols
MESA+ Institute for Nanotechnology
Mesoscale Chemical Systems
Meander 151
University of Twente
Postbus 217
7500 AE Enschede
The Netherlands

Office: +31 (0)53 489 26 31
Mobile: +31 (0)6 49 312 471
Fax   : +31 (0)53 489 35 95
Email : [email protected]
Web   : http://mcs.tnw.utwente.nl/

> From: Moshe 
> Reply-To: General MEMS discussion 
> Date: Tue, 22 Jul 2008 22:55:44 -0700 (PDT)
> To: 
> Subject: Re: [mems-talk] Gold Etchant with selectivity over Mo
>
> I know that Aqua Regia may etch gold but I don't know what it influence on the
> Mo.
> Aqua regia composition : 25% concentration  HNO3 + 75% concentration    HCl
> It is very corrosive solution, please be careful!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation