A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: SU-8
Re: SU-8
1998-08-20
Louis Guerin
1998-08-21
Hubert Lorenz
1998-08-25
Fred Tepper
1998-10-22
Louis Guerin
1998-10-22
[email protected]
1998-10-22
Xing Yang
1998-10-23
Louis Guerin
1998-10-22
[email protected]
Re: SU-8
[email protected]
1998-10-22
Hi

There is an article published in IEEE MEMS 1998 Proceedings
that deals with SU-8.
 "Taguchi Optimization for the processing Epon SU-8 resist"
 B.Eyre,J.Blosiu and D.Wiberg
 Center for Space Microelectronics Technology
 Jet Propulsion Laboratory
 California Institute of Technology
 Pasadena,CA 91109

Optimized process variables such as softbake time,exposure time,
post-exposure time,develop time and sustrate type for SU-8 with
73% solvent was obtained.

Hope this could be of help.

Regan Nayve


Zeng Yi wrote:
>
> Dear Members:
>      I am new student in MEMS. Now I am concerning to use SU-8
> photoresist for some microstructures. But I do not know how to
> control the depth of the SU-8 layer? Could anyone tell me something
> about that? Thank you for your time and consideration.
> Zeng Yi
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
Nano-Master, Inc.