A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: how to drill a hole in a silicon wafer
how to drill a hole in a silicon wafer
2010-12-05
Petru Lunca Popa
2010-12-06
Xiaohui Lin
2010-12-07
shimul saha
2010-12-06
Kuijpers, Peter
2010-12-06
Shay Kaplan
2010-12-07
Nabhiraj Yalagoud
2010-12-07
Andrew Sarangan
2010-12-09
Nabhiraj Yalagoud
2010-12-09
Ned Flanders
2010-12-10
Gomez, Mikel
how to drill a hole in a silicon wafer
Xiaohui Lin
2010-12-06
ultra sonic drilling can be use to drill 1mm hole on wafers

On Sun, Dec 5, 2010 at 12:39 PM, Petru Lunca Popa  wrote:

> Hi,
>
> I have just an ordinary Si/SiO2 commercial wafer and I want to to
> put a hole in it . The shape is not so important. Area should be around one
> mm squared or less.
>
> Any ideea how to do this without breaking the wafer?
> Mechanical or chemical methods?
>
> Thank you
> Petru

--
Lin, Xiaohui
Ph.D. Program in Electrical and Computer Engineering
Nanophotonics and Optical Interconnects Group
Microelectronics Research Center
The University of Texas at Austin
E-mail: [email protected]
Office: (512) 471-4349
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics