A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: dilute SU-8 2075
dilute SU-8 2075
2011-04-20
첸로
2011-04-20
[email protected]
2011-04-20
Jon R. Fox
2011-04-21
첸로
2011-04-20
Kevin Nichols
2011-04-21
첸로
2011-04-21
Kevin Nichols
2011-04-22
첸로
2011-04-21
Jin Yu
2011-04-21
Mike Stan
dilute SU-8 2075
Jin Yu
2011-04-21
You can use PGMEA to dilute SU-8

Regards,

Jin



-----Original Message-----
From: 첸로 [mailto:[email protected]]
Sent: 20 April 2011 12:10
To: mems-talk
Subject: [mems-talk] dilute SU-8 2075


Dear everyone,

I am using SU-8 2075 in photolithography. I want to get a thin film after spin
coating so i intend to use IPA to dilute su-8, but it does not work. Has anybody
encountered this problem?  How do you dilute the su-8?

Any suggestion will be highly appreciated.

Thanks in advance.
Regards
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics