PDMS surface hydrophobic property
righeira carnegie
2011-05-02
Hi again,

Instead of O2 plasma, try using the mixture of SF6 + 02 with various
composition.  I would suggest equal proportion first then try increasing the
volume of SF6. Maybe it works.

regards