MEMSnet Home: MEMS-Talk: PDMS surface hydrophobic property
PDMS surface hydrophobic property
2011-05-01
첸로
2011-05-02
righeira carnegie
2011-05-02
righeira carnegie
2011-05-02
righeira carnegie
2011-05-03
첸로
PDMS surface hydrophobic property
righeira carnegie
2011-05-02
ok it is SiF4(silicon tetra flouride) +O2 not SF6 :)