Hi,

One thing I learned is that Kapton bond to almost nothing.

One of our group member used to do Si/PDMS bonding and she suffered a
problem that the PDMS also bond to a copper fixture she used to apply
pressure on it. I suggested her to tape kapton on the fixture to
isolate the PDMS from the fixture because kapton is something don't
adhere and can sustain the temperature. It works.

Best



2011/7/25 Shane GUO :
> Hello everyone,
>
> I searched old posts about addressing this issue without any luck. Basically,
I have a Kapton sheet with electrodes on it and try to bond it with PDMS. I
found PDMS does not adhere to Kapton to form a stable bonding. Both PDMS and
Kapton are cleaned with acetone, IPA and DI water, dried and treated with O2
plasma for 1min and 5mins respectively. Can anyone shed some light on me?
>
> Cheers

--
Yunda Wang, Ph.D. Candidate
Department of Mechanical engineering
University of Colorado - Boulder
Boulder,Co. US. 80302
(614)3120920
E-mail: [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics