Hi,

I dont think you ll succeed in sticking because for a stable bonding you
will need some Si OH bonds to be activated by plasma. No Si in your kapton
so no Si bond. Try to put some Si O2 on the kapton and then should work.
Good luck . You ll need it.

Petru

La data de , Shane GUO  a scris:
> Hello everyone,

> I searched old posts about addressing this issue without any luck.
> Basically, I have a Kapton sheet with electrodes on it and try to bond it
> with PDMS. I found PDMS does not adhere to Kapton to form a stable
> bonding. Both PDMS and Kapton are cleaned with acetone, IPA and DI water,
> dried and treated with O2 plasma for 1min and 5mins respectively. Can
> anyone shed some light on me?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Addison Engineering
University Wafer