NR2-20000P on Copper
Ricky Anthony
2013-09-20
Hi All,

I have been testing this chemically amplified negative tone photoresist on
copper for some time now. I have found that:


1.       There is adhesion issue between Copper and the resist. Does anyone know
the reason behind it.

2.       The dedicated developer RD6 shows leaves marks on the copper. As though
because of contamination. Does anyone know how to over come this. I am working
in a completely metal-ion free bench.

Many Thanks,
Ricky
Tyndall National Institute
Cork, Ireland
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
Addison Engineering
Process Variations in Microsystems Manufacturing