A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: AZ9260 double spinning recipe
AZ9260 double spinning recipe
2013-10-03
Orozaliev Ajymurat Nurdinovich
2013-10-03
basar bolukbas
2013-10-03
Jonathan Lueke
2013-10-06
Orozaliev Ajymurat Nurdinovich
2013-10-03
Gary Hillman
2013-10-04
Alex Feldman
2013-10-04
Ioannis Nikolaou
2013-10-04
Orozaliev Ajymurat Nurdinovich
2013-10-06
Ioannis Nikolaou
AZ9260 double spinning recipe
Orozaliev Ajymurat Nurdinovich
2013-10-03
Hi All,

I was working on thick AZ9260 resist for using as a mask on DRIE tool.
My target is to etch 450-480 um of Silicon. I have preliminary results for
PR:Si selectivity, which is ~1:25. To etch 450 um of Si, I would need at
least 18 um(but more the better) of AZ9260. With single coating I am
getting maximum of 15 um. But when I do double spinning and expose it, the
resist is turning yellowish-orange. Further, I develope it, but when I put
it inside the DRIE tool, after a few cycles, the resist is forming flakes
and contaminating inside the chamber.

Here is my recipe:
-2000 rpm - 60 s
-removing edge bead with Acetone, while spinning.
-Soft bake at 110 C for 90 s
-2000 rpm - 60 s
-Soft bake at 110 C for 240 s.

-Exposure, broadband source,950 mJ/cm2.
-Developer, AZ400:DI 4:1, 3-4 mins.
With this recipe, I am getting ~25 um. but when I put it inside DRIE,the
resist is just peeling of and forming flakes.

Can you please advise if there is something I am missing?
Also, any recipe would be much appreciated.

kind regards,
Ajymurat
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics