MEMSnet Home: MEMS-Talk: How to make a metal grid
How to make a metal grid
2016-07-05
John Bohland
2016-07-06
Bill Moffat
2016-07-06
Bill Moffat
2016-07-06
Gary Hillman
2016-07-06
[email protected]
2016-07-07
Philipp Altpeter
2016-07-07
Wilson, Thomas
2016-07-07
Andrew Sarangan
2016-07-12
Daniel Figura
2016-07-12
Roberto Igal Chertkow
2016-07-13
John Bohland
How to make a metal grid
Gary Hillman
2016-07-06
John, photolithographic technology is the clear answer to your question. Gary



Gary Hillman
S-Cubed
9 Mars Court ( USPS PO Box 365)
Montville, NJ 07045

Phone 973-263-0640 ex 535
Mobile 201-755-3760



________________________________________
From: [email protected] [mems-talk-
[email protected]] on behalf of John Bohland
[[email protected]]
Sent: Tuesday, June 28, 2016 8:56 PM
To: [email protected]
Subject: [mems-talk] How to make a metal grid

I am interested in making a metal grid on a 370 mm X 470 mm glass substrate.

The problem is that the metallization lines must be only 1.5 microns in width
and spaced (pitch) only a few microns apart.

The metal can be Al or Ag and 100 nm thick.

The best idea I have is to monolithically coat the glass with sputtered (PVD) Al
or Ag then use a picoseond laser to remove all but the desired 1.5 micron wide
metal line widths. Even then I don't know if the laser would have good enough
resolution to meet these requirements.

Anyone have better ideas?

Thanks,

John

NOTICE
This transmittal and/or attachments ("Communication") is confidential to Bloo
Solar, or may otherwise be privileged information. If you are not the intended
recipient, you are hereby notified that you have received this Communication in
error and any dissemination, distribution or copying of this Communication is
strictly prohibited. If you have received this Communication in error, please
notify us immediately and promptly delete and purge this Communication.

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics