MEMSnet Home: MEMS-Talk: How to make a metal grid
How to make a metal grid
2016-07-05
John Bohland
2016-07-06
Bill Moffat
2016-07-06
Bill Moffat
2016-07-06
Gary Hillman
2016-07-06
[email protected]
2016-07-07
Philipp Altpeter
2016-07-07
Wilson, Thomas
2016-07-07
Andrew Sarangan
2016-07-12
Daniel Figura
2016-07-12
Roberto Igal Chertkow
2016-07-13
John Bohland
How to make a metal grid
Bill Moffat
2016-07-06
Additional information on Lift Off. Cray research manufactured their own chips
at Chippewa Falls and used Image Reversal to produce 0.1 micron metal lines in
production. The best dimensional control I have seen is 0.08 micron lines and
spaces. This was because the mask dimensions were limited to 0.08 microns. Bill
Moffat

-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of Bill Moffat
Sent: Tuesday, July 05, 2016 3:21 PM
To: General MEMS discussion
Subject: Re: [mems-talk] How to make a metal grid

Far simpler to put down resist pattern then metalize and lift off metal. For
micron and sub-micron metal easiest and least expensive. Bill Moffat

-----Original Message-----
From: [email protected] [mailto:mems-
[email protected]] On Behalf Of John Bohland
Sent: Tuesday, June 28, 2016 5:57 PM
To: [email protected]
Subject: [mems-talk] How to make a metal grid

I am interested in making a metal grid on a 370 mm X 470 mm glass substrate.

The problem is that the metallization lines must be only 1.5 microns in width
and spaced (pitch) only a few microns apart.

The metal can be Al or Ag and 100 nm thick.

The best idea I have is to monolithically coat the glass with sputtered (PVD) Al
or Ag then use a picoseond laser to remove all but the desired 1.5 micron wide
metal line widths. Even then I don't know if the laser would have good enough
resolution to meet these requirements.

Anyone have better ideas?

Thanks,

John

NOTICE
This transmittal and/or attachments ("Communication") is confidential to Bloo
Solar, or may otherwise be privileged information. If you are not the intended
recipient, you are hereby notified that you have received this Communication in
error and any dissemination, distribution or copying of this Communication is
strictly prohibited. If you have received this Communication in error, please
notify us immediately and promptly delete and purge this Communication.

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics