MEMSnet Home: MEMS-Talk: Re: Etching Teflon
Re: Etching Teflon
1999-03-11
Fred Tepper
1999-03-11
Alexander Shenderov
1999-03-11
Jonathan Bernstein
1999-03-11
Fred Tepper
1999-03-11
Yohannes
1999-03-23
[email protected]
Re: Etching Teflon
Fred Tepper
1999-03-11
This is a multi-part message in MIME format.
--------------9A0053D5232DFC40632C2240
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

I seem to recall that a sodium metal dispersion in a hydrocarbon is being sold
and
used for etching teflon.  I don't recall who the manufacturer is.

Robert Okojie wrote:

> Folks,
>
> I am compiling information on Teflon, but the etching characteristics have
been
> particularly elusive.
>
> Can anyone help in this regard?  Information on its molding will also be
> appreciated.
>
> Thank you.
>
> Robert.
>
> --
> Robert S. Okojie, Ph.D.
> Senior Engineer
> Ford Microelectronics
> 9965 Federal Drive, Colorado Springs, CO 80921-3698
> Phone:(719)528-7727; Fax: (719)528-7529
> "The frontier of knowledge has no boundary.  Paradigms rise and fall"
>

--------------9A0053D5232DFC40632C2240
Content-Type: text/x-vcard; charset=us-ascii;
 name="fred.vcf"
Content-Transfer-Encoding: 7bit
Content-Description: Card for Fred Tepper
Content-Disposition: attachment;
 filename="fred.vcf"

begin:vcard
n:Tepper;Fred
x-mozilla-html:FALSE
adr;dom;quoted-printable:;;240  Power Court=0D=0ASuite 108;Sanford;Fl;32771;
org:Argonide Corp - www.argonide.com
version:2.1
email;internet:[email protected]
title:President - 407-322-2500
tel;fax:322-1144
tel;work:407-322-2500
x-mozilla-cpt:;0
fn:Fred Tepper
end:vcard

--------------9A0053D5232DFC40632C2240--


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review