Re: Etching Teflon
Yohannes
1999-03-11
At 05:34 PM 3/8/99 -0700, you wrote:
>Folks,
>
>I am compiling information on Teflon, but the etching characteristics have
been
>particularly elusive.
>
>Can anyone help in this regard?  Information on its molding will also be
>appreciated.
>
>Thank you.
>
>Robert.
>

Hi Robert,

You might be interested to know that teflon is sensitive to x-ray
radiaiton.  When exposed to x-ray radiation.  I'm not sure about the rate
but I think it is about 10 microns/minute.  If you want more information,
let me know.

Regards,
Yohannes


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing