Re: selective etching of Cu (Ag) over alumina
[email protected]
1999-05-05
A company named Southwest microelectronicws materials in Az makes a gold etch
solution that will etch copper also. Ask for turkey blood and it is a iodine
solution, Ask for Mike Dodd. Phone is 480-885-1020.  Tell him Bob Henderson
sent you.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.