Piezoresistor simulation
A.J Pang
2002-06-18
Hi YanJun,

I don't think you can model and simulate a piezoresistive effect using the
piezoelectric element of ANSYS!

what you can do is to try and model a diaphragm, apply the stress or pressure on
it, then read out the stress on the diaphragm and convert it into output voltage
using the piezoresistive equations.

hope this help.

AJ Pang


----- Original Message -----
From: "Yuan-Fang Chou" 
To: 
Sent: Tuesday, June 18, 2002 2:50 AM
Subject: Re: [mems-talk] Piezoresistor simulation


> Yanjun,
>
> There is a paper that you might be interested in. It is
>
> Chou, Yuan-Fang, and Lin, Rong-Sheng,  "Optimization for Piezoresistor
> Design," Proceedings of the 13th European Conference on Solid-State Sensors,
> Actuators and Microsystems , pp. 65-68, The Netherlands, 1999.
>
> Yuan-Fang
>
>
> ----- Original Message -----
> From: "Yanjun(David) Tang" 
> To: 
> Sent: Monday, June 17, 2002 10:43 AM
> Subject: [mems-talk] Piezoresistor simulation
>
>
> > Hello, folks
> >  I am doing piezoresistor simulation in MEMS using the program ANSYS. Do
> you
> > have some clues about what kind of couple-field element in Ansys can
> account
> > for the interaction between displacement of element ( the displacemetn
> induces
> > stress and stress induces strain of element then), and the change of its
> > resistivity. The piezoelectric element only  reflects how structural
> > displacement affect voltage distribution.
> > Thanks
> >
> > Yanjun Tang
> >
> > Louisiana Tech Univeristy
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe or change your list
> > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS processing services.
> > Visit us at http://www.memsnet.org/
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Addison Engineering