CMOS Complementary metal oxide semiconductor - integrated circuit containing n-channel and p-channel MOSFETs.
Codons Organic bases in sets of three that form the genetic code.
Conductor Material such as the metals copper or aluminum that conducts electricity via the motion of electrons.
Copolymer A polymer that consists of two or more dissimilar monomer units in combination in its molecular chains. Also a polymer formed from the polymerization of more than one type of monomer.
Corrosion Deteriorative loss of a metal as a result of dissolution environmental reactions.
Coulomb [C] Measure of electrical charge: 1 C is an amount of charge equal to that of about 6.24x1018 electrons.
Covalent bond A primary interatomic bond that is formed by the sharing of electrons between neighboring atoms.
Creep The time-dependent permanent deformation that occurs under stress; for most materials it is important only at elevated temperatures.
Cross-sensitivity The influence of one measurand on the sensitivity of a sensor, another measurand.
Crosslinked polymer A polymer in which adjacent linear molecular chains are joined at various positions by covalent bonds.
Results Page:  1 2 3 4 5 6 7 8 9 10 > >|
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
Addison Engineering