Adhesion promoter between gold and PMMA
2006-01-11
Thomas Kiefer
2006-01-11
[email protected]
2006-01-11
sokwon Paik
2006-01-11
Loren St. Clair
Adhesion promoter between gold and PMMA
[email protected]
2006-01-11
There is a procedure using HMDS and another linker that can be released.

Sorry for the last email my figure slipped and hit send.

> Hi,
>
> does anyone know a good adhesion promoter for PMMA on gold?
> I'm using 35k PMMA, spin-coated on a thin gold layer. I'd like to
> avoid using other metals to improve the adhesion. It should also be
> possible to remove the adhesion promoter later easily.
>
> Thomas,
> EPFL, Lausanne
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation