Adhesion promoter between gold and PMMA
Loren St. Clair
2006-01-11
Sokwon,

Could you please give a short summary of the paper?  I appreciate your help,

Loren St. Clair

 -----Original Message-----
From:   [email protected] [mailto:[email protected]]  On
Behalf Of sokwon Paik
Sent:   Wednesday, January 11, 2006 11:27 AM
To:     General MEMS discussion
Subject:        Re: [mems-talk] Adhesion promoter between gold and PMMA

Thomas,

  Journal of Vaccum science Technol. B 1998 16 (6) 3543-3546 could be the good
source for your refrerence.

  Good luck,

  Sokwon
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
The Branford Group
Process Variations in Microsystems Manufacturing