2006-05-24
g.balsubra manian
2006-05-24
Gareth Jenkins
PDMS pull test.
g.balsubra manian
2006-05-24
Hi Experts and Guys.,

Good morning. I am doing PDMS bonding at various
conditions and interested in doing pull test of PDMS
/Si wafer.

I have to stick PDMS with Al soccle (holder) inorder
to perform Pull test. Tha adhesion between PDMS and Al
soccle should be better than between PDMS and Si
inorder to do pull test.

What/Which glue can be used to get a better adhesion
of PDMS with Al??.

Thanks
Bala.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.