MEMSnet Home: MEMS-Talk: PDMS pull test.
PDMS pull test.
2006-05-24
g.balsubra manian
2006-05-24
Gareth Jenkins
PDMS pull test.
Gareth Jenkins
2006-05-24
g.balsubra manian wrote:

>What/Which glue can be used to get a better adhesion
>of PDMS with Al??.
>
>
Why not use (uncured) PDMS itself?
It should stick well enough to Al and irreversibly to PDMS.