A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Silicon_Glass Fusion Bonding
Silicon_Glass Fusion Bonding
2009-02-10
jingru zhang
2009-02-10
Joseph Grogan
2009-02-10
jingru zhang
2009-02-10
Bill Moffat
2009-02-10
Xiaoguang Liu
2009-02-10
Bill Moffat
2009-02-10
jingru zhang
2009-02-11
Shay Kaplan
2009-02-11
Joseph Grogan
2009-02-12
Brubaker Chad
2009-02-12
shay kaplan
2009-02-12
Gareth Jenkins
2009-02-12
Roger Shile
2009-02-13
jingru zhang
2009-02-13
Roger Shile
2009-02-13
Reza Rashidi
2009-02-13
Joseph Grogan
Silicon_Glass Fusion Bonding
Bill Moffat
2009-02-10
Do you have plasma equipment?  Plasma bonding is possible.  Bill Moffat

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of jingru zhang
Sent: Tuesday, February 10, 2009 10:12 AM
To: [email protected]
Subject: [mems-talk] Silicon_Glass Fusion Bonding

Dear all,

Since we don't have equipment for anodic bonding in the lab, I need to
figure out how to bond silicon and glass together by fusion bonding?
However, I tried lots of pieces and they all failed. I did HF and RCA 1
clean for both silicon substrate (with pattern on it) and glass before
bonding but it 's not bonding. Does anyone have done silicon and glass
fusion bonding before? Any suggestions will be appreciated.

Thank you.

Best,
Jingru
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Harrick Plasma, Inc.