MEMSnet Home: MEMS-Talk: Silicon_Glass Fusion Bonding
Silicon_Glass Fusion Bonding
2009-02-10
jingru zhang
2009-02-10
Joseph Grogan
2009-02-10
jingru zhang
2009-02-10
Bill Moffat
2009-02-10
Xiaoguang Liu
2009-02-10
Bill Moffat
2009-02-10
jingru zhang
2009-02-11
Shay Kaplan
2009-02-11
Joseph Grogan
2009-02-12
Brubaker Chad
2009-02-12
shay kaplan
2009-02-12
Gareth Jenkins
2009-02-12
Roger Shile
2009-02-13
jingru zhang
2009-02-13
Roger Shile
2009-02-13
Reza Rashidi
2009-02-13
Joseph Grogan
Silicon_Glass Fusion Bonding
Xiaoguang Liu
2009-02-10
Hi Bill
Could you elaborate on the plasma bonding process?
Thanks,
Leo

On Tue, Feb 10, 2009 at 3:00 PM, Bill Moffat
 wrote:
> Do you have plasma equipment?  Plasma bonding is possible.  Bill Moffat
>

Xiaoguang "Leo" Liu
Birck Nanotechnology Center,
Purdue University,
1205 W.State Street, West Lafayette, IN, 47906 USA
[email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing