MEMSnet Home: MEMS-Talk: Bubbles in my SU-8
Bubbles in my SU-8
2003-03-14
frank berisford
2003-03-17
Christopher F. Blanford
2003-03-17
Jennifer Pagan
2003-03-17
Josef Kouba
2003-03-18
Mark Shaw
heat effect on MUMPS cantilever beam
2003-04-04
weiwei2
Bubbles in my SU-8
Christopher F. Blanford
2003-03-17
Dear Frank Berisford

I put the SU-8 resist into a sonic bath with a degas cycle to removed
dissolved gases. This cycle pulses the sonics, assisting the nucleation
of these gases. About 5 minutes of pulsed sonics at full power and 40
C, gives (nearly) bubble-free coatings.

Regards,

Chris Blanford

On Friday, March 14, 2003, at 11:07  am, frank berisford wrote:

> I've been trying several different techniques in an attempt to
> minimize bubbles
> in my SU-8.  At first I tried pippeting it onto my substrate using a
> large bore
> pippette.  I also tried dispensing from a syringe and pouring straight
> from
> the bottle.  The pouring seems to work best but I still get a sizable
> bubble
> count.  From here I've tried sucking the bubbles out with a needle and
> syringe
> but to no avail.
--
Christopher F. Blanford
Inorganic Chemistry Laboratory, South Parks Road, Oxford, OX1 3QR, UK
Phone: +44 (0)1865 282603; Fax: +44 (0)1865 272690
PGP keyID: 8D830BC9  http://pgp.mit.edu/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation