A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Looking for mask to make holes in glass
Looking for mask to make holes in glass
2009-03-04
Moshe
2009-03-04
John Dangtran
2009-03-06
Albert Henning
2009-03-04
Mehmet Aykol
2009-03-04
Andrea Mazzolari
2009-03-04
Hanson, Steve
2009-03-06
Zhao Lu
2009-03-09
Mikael Evander
2009-03-05
Moshe
2009-03-05
walter
2009-03-05
Fei Wang
2009-03-06
Morten Aarøe
2009-03-06
Pat Kayatta
2009-03-06
akshdeep sharma
Looking for mask to make holes in glass
Moshe
2009-03-04
Hello

I am looking for a way to make holes 1 mm diameter in glass.
I did gold mask on the glass and  tried polysilicon as a mask too but the HF
stripped the masks.

Do you have a solution for the mask ?

Thank you



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.