A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Looking for mask to make holes in glass
Looking for mask to make holes in glass
2009-03-04
Moshe
2009-03-04
John Dangtran
2009-03-06
Albert Henning
2009-03-04
Mehmet Aykol
2009-03-04
Andrea Mazzolari
2009-03-04
Hanson, Steve
2009-03-06
Zhao Lu
2009-03-09
Mikael Evander
2009-03-05
Moshe
2009-03-05
walter
2009-03-05
Fei Wang
2009-03-06
Morten Aarøe
2009-03-06
Pat Kayatta
2009-03-06
akshdeep sharma
Looking for mask to make holes in glass
Mehmet Aykol
2009-03-04
If you are trying to make holes then you can use a diamond coated drill bit.

Mehmet

On Wed, Mar 4, 2009 at 10:23 AM, Moshe  wrote:

> Hello
>
> I am looking for a way to make holes 1 mm diameter in glass.
> I did gold mask on the glass and  tried polysilicon as a mask too but the
> HF stripped the masks.
>
> Do you have a solution for the mask ?
>
> Thank you

--
Mehmet Aykol
University of Southern California
EE - Electrophysics
Phone: (213) 821-4090
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review
Nano-Master, Inc.