MEMSnet Home: MEMS-Talk: Looking for mask to make holes in glass
Looking for mask to make holes in glass
2009-03-04
Moshe
2009-03-04
John Dangtran
2009-03-06
Albert Henning
2009-03-04
Mehmet Aykol
2009-03-04
Andrea Mazzolari
2009-03-04
Hanson, Steve
2009-03-06
Zhao Lu
2009-03-09
Mikael Evander
2009-03-05
Moshe
2009-03-05
walter
2009-03-05
Fei Wang
2009-03-06
Morten Aarøe
2009-03-06
Pat Kayatta
2009-03-06
akshdeep sharma
Looking for mask to make holes in glass
akshdeep sharma
2009-03-06
Hello Dear,

May be you can Try milling machine for making a hole in a glass wafer.  Earlier
i
used it for making a hole in glass wafer.

Best Regard
Akshdeep Sharma
Project Assistant
Sensors & Nanotechnology Group
CEERI Pilani
Mob.+919828778852
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing
MEMS Technology Review