MEMSnet Home: MEMS-Talk: Looking for mask to make holes in glass
Looking for mask to make holes in glass
2009-03-04
Moshe
2009-03-04
John Dangtran
2009-03-06
Albert Henning
2009-03-04
Mehmet Aykol
2009-03-04
Andrea Mazzolari
2009-03-04
Hanson, Steve
2009-03-06
Zhao Lu
2009-03-09
Mikael Evander
2009-03-05
Moshe
2009-03-05
walter
2009-03-05
Fei Wang
2009-03-06
Morten Aarøe
2009-03-06
Pat Kayatta
2009-03-06
akshdeep sharma
Looking for mask to make holes in glass
Zhao Lu
2009-03-06
Hello,

I tried diamond drill bits on Pyrex and glass slides. It worked well. Just drill
it slowly without too much pressure. Put a drop of water on the drilling site
will greatly smooth the wall of the hole.


Zhao

Quoting Moshe :

> Hello
>
> I am looking for a way to make holes 1 mm diameter in glass.
> I did gold mask on the glass and  tried polysilicon as a mask too but the HF
> stripped the masks.
>
> Do you have a solution for the mask ?
>
> Thank you

     Zhao Lu
     École Polytechnique de Montréal
     Lassonde Building room M-4505
     Campus of University of Montreal
     Montréal, Qc, Canada
     H3T 1J4
     Tel 514-340-4711 ext 5029
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics